{"_buckets": {"deposit": "94f9e5ee-e2ae-4ac0-b84f-c242cefa2763"}, "_deposit": {"created_by": 3, "id": "12988", "owners": [3], "pid": {"revision_id": 0, "type": "depid", "value": "12988"}, "status": "published"}, "_oai": {"id": "oai:sucra.repo.nii.ac.jp:00012988", "sets": ["426"]}, "author_link": ["20668", "20667", "20666", "18337", "20669"], "item_119_alternative_title_1": {"attribute_name": "タイトル(別言語)", "attribute_value_mlt": [{"subitem_alternative_title": "Corrosion of Sintered High-Purity Mullite in Molten KF Salt"}]}, "item_119_biblio_info_8": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "1992", "bibliographicIssueDateType": "Issued"}, "bibliographicIssueNumber": "1164", "bibliographicPageEnd": "1014", "bibliographicPageStart": "1011", "bibliographicVolumeNumber": "100", "bibliographic_titles": [{"bibliographic_title": "日本セラミックス協会学術論文誌"}]}]}, "item_119_date_31": {"attribute_name": "作成日", "attribute_value_mlt": [{"subitem_date_issued_datetime": "2008-01-09", "subitem_date_issued_type": "Created"}]}, "item_119_description_17": {"attribute_name": "関連サイト", "attribute_value_mlt": [{"subitem_description": "http://ci.nii.ac.jp/naid/110002290063/ | http://ci.nii.ac.jp/naid/110002290063/", "subitem_description_type": "Other"}]}, "item_119_description_19": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": "Corrosion behaviors of sintered mullite bodies (99% in RD) with spherical and columnar shapes fabricated from high-purity mullite powders synthesized using a sol-gel processing have been investigated at 900℃, 950℃ and 1000℃ for 5-180 min in KF melt. For both shapes, the reaction of the sintered mullite bodies with KF melt proceeded from the entire surface bodies towards the inner part uniformly at the interface. The thickness of corrosion layer formed at the interface increased relatively uniformly with increases in dipping temperature and time, and it was revealed that the corrosion proceeds parabolically. The corrosion layer acted as a protective layer against the corrosion reaction and suppressed the subsequent corrosion reaction. Using a geometrical shape-parameter depending on the initial sample shape, the process of corrosion progress could be expressed in terms of the diffusion controlled reaction rate equation based on the unreacted core model through the reaction layer.", "subitem_description_type": "Abstract"}]}, "item_119_description_21": {"attribute_name": "注記", "attribute_value_mlt": [{"subitem_description": "rights: 社団法人日本セラミックス協会\nrights: 本文データは学協会の許諾に基づきCiNiiから複製したものである\nrelation: IsVersionOf: http://ci.nii.ac.jp/naid/110002290063/", "subitem_description_type": "Other"}]}, "item_119_description_29": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"subitem_description": "text", "subitem_description_type": "Other"}]}, "item_119_description_30": {"attribute_name": "フォーマット", "attribute_value_mlt": [{"subitem_description": "application/pdf", "subitem_description_type": "Other"}]}, "item_119_publisher_11": {"attribute_name": "出版者名", "attribute_value_mlt": [{"subitem_publisher": "社団法人日本セラミックス協会"}]}, "item_119_relation_7": {"attribute_name": "著者 外部リンク", "attribute_value_mlt": [{"subitem_relation_name": [{"subitem_relation_name_text": "\u0026EMPTY\u0026"}], "subitem_relation_type_id": {"subitem_relation_type_id_text": "\u0026EMPTY\u0026", "subitem_relation_type_select": "URI"}}, {"subitem_relation_name": [{"subitem_relation_name_text": "\u0026EMPTY\u0026"}], "subitem_relation_type_id": {"subitem_relation_type_id_text": "\u0026EMPTY\u0026", "subitem_relation_type_select": "URI"}}, {"subitem_relation_name": [{"subitem_relation_name_text": "http://s-read.saitama-u.ac.jp/researchers/pages/researcher/QNzSsZBx"}], "subitem_relation_type_id": {"subitem_relation_type_id_text": "http://s-read.saitama-u.ac.jp/researchers/pages/researcher/QNzSsZBx", "subitem_relation_type_select": "URI"}}]}, "item_119_source_id_14": {"attribute_name": "ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "09145400", "subitem_source_identifier_type": "ISSN"}]}, "item_119_text_27": {"attribute_name": "版", "attribute_value_mlt": [{"subitem_text_value": "[出版社版]"}]}, "item_119_text_3": {"attribute_name": "著者 ローマ字", "attribute_value_mlt": [{"subitem_text_value": "MITAMURA, Takashi"}, {"subitem_text_value": "MASUDA, Tomoyuki"}, {"subitem_text_value": "KOBAYASHI, Hidehiko"}, {"subitem_text_value": "KATAYAMA, Keiichi"}, {"subitem_text_value": "AKIBA, Tokuji"}]}, "item_119_text_32": {"attribute_name": "アイテムID", "attribute_value_mlt": [{"subitem_text_value": "A1002237"}]}, "item_119_text_35": {"attribute_name": "公開日(XooNIps)", "attribute_value_mlt": [{"subitem_text_value": "Jan 9, 2008 09:00:00"}]}, "item_119_text_36": {"attribute_name": "最終更新日(XooNIps)", "attribute_value_mlt": [{"subitem_text_value": "Sep 8, 2009 12:04:42"}]}, "item_119_text_37": {"attribute_name": "更新履歴(XooNIps)", "attribute_value_mlt": [{"subitem_text_value": "Sep 8, 2009 フリーキーワード, 著者 を変更"}, {"subitem_text_value": "Mar 17, 2009 フリーキーワード, キーワード を変更"}, {"subitem_text_value": "Oct 8, 2008 フリーキーワード, インデックス, キーワード を変更"}, {"subitem_text_value": "Aug 8, 2008 フリーキーワード, キーワード を変更"}, {"subitem_text_value": "Feb 27, 2008 フリーキーワード, インデックス, キーワード を変更"}, {"subitem_text_value": "Feb 2, 2008 フリーキーワード, インデックス, キーワード を変更"}, {"subitem_text_value": "Jan 31, 2008 フリーキーワード, インデックス, キーワード を変更"}, {"subitem_text_value": "Jan 9, 2008 コメント, ID, フリーキーワード, インデックス, 版, キーワード を変更"}]}, "item_119_text_38": {"attribute_name": "登録者(XooNIps)", "attribute_value_mlt": [{"subitem_text_value": "sucra_jim4"}]}, "item_119_text_39": {"attribute_name": "閲覧数(XooNIps)", "attribute_value_mlt": [{"subitem_text_value": "1416"}]}, "item_119_text_4": {"attribute_name": "著者 所属", "attribute_value_mlt": [{"subitem_text_value": "埼玉大学工学部"}, {"subitem_text_value": "埼玉大学工学部応用化学科"}, {"subitem_text_value": "埼玉大学大学院理工学研究科物質科学部門"}, {"subitem_text_value": "秩父セメント(株)ファインセラミックス本部"}, {"subitem_text_value": "秩父セメント(株)ファインセラミックス本部"}]}, "item_119_text_40": {"attribute_name": "ダウンロード数(XooNIps)", "attribute_value_mlt": [{"subitem_text_value": "472"}]}, "item_119_text_41": {"attribute_name": "XooNIps_インデックス", "attribute_value_mlt": [{"subitem_text_value": "sucra_jim4|Public/埼玉大学/理工学研究科|Public/埼玉大学/理工学研究科/物質科学部門|Public/主題別/化学/材料化学/無機工業材料|Public/ジャンル別/学術雑誌論文(国内)/日本セラミックス協会"}]}, "item_119_text_42": {"attribute_name": "XooNIps_ITEM_KEY", "attribute_value_mlt": [{"subitem_text_value": "1426"}]}, "item_119_text_5": {"attribute_name": "著者 所属(別言語)", "attribute_value_mlt": [{"subitem_text_value": "Faculty of Engineering, Saitama University"}, {"subitem_text_value": "Department of Applied Chemistry, Faculty of Engineering, Saitama University"}, {"subitem_text_value": "Department of Applied Chemistry, Faculty of Engineering, Saitama University"}, {"subitem_text_value": "Department of Fine Ceramics, Chichibu Cement Co.. Lid."}, {"subitem_text_value": "Department of Fine Ceramics, Chichibu Cement Co.. Lid."}]}, "item_119_text_9": {"attribute_name": "年月次", "attribute_value_mlt": [{"subitem_text_value": "1992-8"}]}, "item_119_version_type_28": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_version_resource": "http://purl.org/coar/version/c_970fb48d4fbd8a85", "subitem_version_type": "VoR"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "三田村, 孝"}, {"creatorName": "ミタムラ, タカシ", "creatorNameLang": "ja-Kana"}], "nameIdentifiers": [{"nameIdentifier": "20666", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "増田, 知之"}, {"creatorName": "マスダ, トモユキ", "creatorNameLang": "ja-Kana"}], "nameIdentifiers": [{"nameIdentifier": "20667", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "小林, 秀彦"}, {"creatorName": "コバヤシ, ヒデヒコ", "creatorNameLang": "ja-Kana"}], "nameIdentifiers": [{"nameIdentifier": "18337", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "片山, 恵一"}, {"creatorName": "カタヤマ, ケイイチ", "creatorNameLang": "ja-Kana"}], "nameIdentifiers": [{"nameIdentifier": "20668", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "秋葉, 徳二"}, {"creatorName": "アキバ, トクジ", "creatorNameLang": "ja-Kana"}], "nameIdentifiers": [{"nameIdentifier": "20669", "nameIdentifierScheme": "WEKO"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2018-01-24"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "A1002237.pdf", "filesize": [{"value": "681.9 kB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensetype": "license_free", "mimetype": "application/pdf", "size": 681900.0, "url": {"label": "A1002237.pdf", "url": "https://sucra.repo.nii.ac.jp/record/12988/files/A1002237.pdf"}, "version_id": "cc9726fd-756d-4ede-a00b-0f89276f76d4"}]}, "item_keyword": {"attribute_name": "キーワード", "attribute_value_mlt": [{"subitem_subject": "Mullite", "subitem_subject_scheme": "Other"}, {"subitem_subject": "KF molten salt", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Corrosion", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Unreacted core model", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Diffusion controlled reaction rate equation", "subitem_subject_scheme": "Other"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "jpn"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "journal article", "resourceuri": "http://purl.org/coar/resource_type/c_6501"}]}, "item_title": "KF融解塩による高純度ムライト焼結体の腐食", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "KF融解塩による高純度ムライト焼結体の腐食"}]}, "item_type_id": "119", "owner": "3", "path": ["426"], "permalink_uri": "https://sucra.repo.nii.ac.jp/records/12988", "pubdate": {"attribute_name": "公開日", "attribute_value": "2008-01-09"}, "publish_date": "2008-01-09", "publish_status": "0", "recid": "12988", "relation": {}, "relation_version_is_last": true, "title": ["KF融解塩による高純度ムライト焼結体の腐食"], "weko_shared_id": -1}
KF融解塩による高純度ムライト焼結体の腐食
https://sucra.repo.nii.ac.jp/records/12988
https://sucra.repo.nii.ac.jp/records/12988c2796d24-2aa9-4cd8-921f-9f346d972cb7
名前 / ファイル | ライセンス | アクション |
---|---|---|
A1002237.pdf (681.9 kB)
|
|
Item type | 学術雑誌論文 / Journal Article(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2008-01-09 | |||||
タイトル | ||||||
タイトル | KF融解塩による高純度ムライト焼結体の腐食 | |||||
言語 | ||||||
言語 | jpn | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Mullite | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | KF molten salt | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Corrosion | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Unreacted core model | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Diffusion controlled reaction rate equation | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_6501 | |||||
資源タイプ | journal article | |||||
タイトル(別言語) | ||||||
その他のタイトル | Corrosion of Sintered High-Purity Mullite in Molten KF Salt | |||||
著者 |
三田村, 孝
× 三田村, 孝× 増田, 知之× 小林, 秀彦× 片山, 恵一× 秋葉, 徳二 |
|||||
著者 ローマ字 | ||||||
MITAMURA, Takashi | ||||||
著者 ローマ字 | ||||||
MASUDA, Tomoyuki | ||||||
著者 ローマ字 | ||||||
KOBAYASHI, Hidehiko | ||||||
著者 ローマ字 | ||||||
KATAYAMA, Keiichi | ||||||
著者 ローマ字 | ||||||
AKIBA, Tokuji | ||||||
著者 所属 | ||||||
埼玉大学工学部 | ||||||
著者 所属 | ||||||
埼玉大学工学部応用化学科 | ||||||
著者 所属 | ||||||
埼玉大学大学院理工学研究科物質科学部門 | ||||||
著者 所属 | ||||||
秩父セメント(株)ファインセラミックス本部 | ||||||
著者 所属 | ||||||
秩父セメント(株)ファインセラミックス本部 | ||||||
著者 所属(別言語) | ||||||
Faculty of Engineering, Saitama University | ||||||
著者 所属(別言語) | ||||||
Department of Applied Chemistry, Faculty of Engineering, Saitama University | ||||||
著者 所属(別言語) | ||||||
Department of Applied Chemistry, Faculty of Engineering, Saitama University | ||||||
著者 所属(別言語) | ||||||
Department of Fine Ceramics, Chichibu Cement Co.. Lid. | ||||||
著者 所属(別言語) | ||||||
Department of Fine Ceramics, Chichibu Cement Co.. Lid. | ||||||
書誌情報 |
日本セラミックス協会学術論文誌 巻 100, 号 1164, p. 1011-1014, 発行日 1992 |
|||||
年月次 | ||||||
1992-8 | ||||||
出版者名 | ||||||
出版者 | 社団法人日本セラミックス協会 | |||||
ISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 09145400 | |||||
関連サイト | ||||||
内容記述タイプ | Other | |||||
内容記述 | http://ci.nii.ac.jp/naid/110002290063/ | http://ci.nii.ac.jp/naid/110002290063/ | |||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | Corrosion behaviors of sintered mullite bodies (99% in RD) with spherical and columnar shapes fabricated from high-purity mullite powders synthesized using a sol-gel processing have been investigated at 900℃, 950℃ and 1000℃ for 5-180 min in KF melt. For both shapes, the reaction of the sintered mullite bodies with KF melt proceeded from the entire surface bodies towards the inner part uniformly at the interface. The thickness of corrosion layer formed at the interface increased relatively uniformly with increases in dipping temperature and time, and it was revealed that the corrosion proceeds parabolically. The corrosion layer acted as a protective layer against the corrosion reaction and suppressed the subsequent corrosion reaction. Using a geometrical shape-parameter depending on the initial sample shape, the process of corrosion progress could be expressed in terms of the diffusion controlled reaction rate equation based on the unreacted core model through the reaction layer. | |||||
注記 | ||||||
内容記述タイプ | Other | |||||
内容記述 | rights: 社団法人日本セラミックス協会 rights: 本文データは学協会の許諾に基づきCiNiiから複製したものである relation: IsVersionOf: http://ci.nii.ac.jp/naid/110002290063/ |
|||||
版 | ||||||
[出版社版] | ||||||
著者版フラグ | ||||||
出版タイプ | VoR | |||||
出版タイプResource | http://purl.org/coar/version/c_970fb48d4fbd8a85 | |||||
資源タイプ | ||||||
内容記述タイプ | Other | |||||
内容記述 | text | |||||
フォーマット | ||||||
内容記述タイプ | Other | |||||
内容記述 | application/pdf | |||||
作成日 | ||||||
日付 | 2008-01-09 | |||||
日付タイプ | Created | |||||
アイテムID | ||||||
A1002237 |