WEKO3
アイテム
{"_buckets": {"deposit": "b4384781-b505-4125-a699-3ce73f102aae"}, "_deposit": {"created_by": 3, "id": "13007", "owners": [3], "pid": {"revision_id": 0, "type": "depid", "value": "13007"}, "status": "published"}, "_oai": {"id": "oai:sucra.repo.nii.ac.jp:00013007", "sets": ["426"]}, "author_link": ["18337", "20738", "20740", "20739"], "item_119_alternative_title_1": {"attribute_name": "タイトル(別言語)", "attribute_value_mlt": [{"subitem_alternative_title": "Influence of Various Atmospheres on the Corrosion Resistance of Si_3N_4 Sintered Bodies against Steel Making Slag and Its Main Components"}]}, "item_119_biblio_info_8": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "1990", "bibliographicIssueDateType": "Issued"}, "bibliographicIssueNumber": "1136", "bibliographicPageEnd": "354", "bibliographicPageStart": "348", "bibliographicVolumeNumber": "98", "bibliographic_titles": [{"bibliographic_title": "日本セラミックス協会学術論文誌"}]}]}, "item_119_date_31": {"attribute_name": "作成日", "attribute_value_mlt": [{"subitem_date_issued_datetime": "2008-01-09", "subitem_date_issued_type": "Created"}]}, "item_119_description_17": {"attribute_name": "関連サイト", "attribute_value_mlt": [{"subitem_description": "http://ci.nii.ac.jp/naid/110002289042/ | http://ci.nii.ac.jp/naid/110002289042/", "subitem_description_type": "Other"}]}, "item_119_description_19": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": "Corrosion of Si_3N_4 sintered bodies against blast furnace slags, converter slags and main components of these slags such as CaO, FeO and MnO_2 has been studied at 1200°-1400℃ for 1-12 h in air, Ar, N2 and O_2-N_2 atmospheres. For Si_3N_4 sintered bodies containing small amounts of Y_2O_3 and Al_2O_3 additives, the corrosion rate increased with increasing pores and glass phase in; sintered bodies. The corrosion behavior of Si_3N_4 sintered bodies against the various salts in Ar, N_2 and O_2-N_2 atmospheres, except for FeO salt, was very stable. In case of less corrosive salts such as blast furnace slag and CaO, the corrosion rate of Si_3N_4 sintered bodies in O_2-N_2 atmospheres increased with increasing O_2 partial pressure up to the air composition, the corrosion rate decreased extremely then above the air composition. In the corrosion of the Si_3N_4 sintered bodies against the various salts, the oxidation of Si3N4 seems to have occurred, and the corrosion proceeded continually by the reaction of SiO_2 with the salts", "subitem_description_type": "Abstract"}]}, "item_119_description_21": {"attribute_name": "注記", "attribute_value_mlt": [{"subitem_description": "rights: 社団法人日本セラミックス協会\nrights: 本文データは学協会の許諾に基づきCiNiiから複製したものである\nrelation: IsVersionOf: http://ci.nii.ac.jp/naid/110002289042/", "subitem_description_type": "Other"}]}, "item_119_description_29": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"subitem_description": "text", "subitem_description_type": "Other"}]}, "item_119_description_30": {"attribute_name": "フォーマット", "attribute_value_mlt": [{"subitem_description": "application/pdf", "subitem_description_type": "Other"}]}, "item_119_publisher_11": {"attribute_name": "出版者名", "attribute_value_mlt": [{"subitem_publisher": "社団法人日本セラミックス協会"}]}, "item_119_relation_7": {"attribute_name": "著者 外部リンク", "attribute_value_mlt": [{"subitem_relation_name": [{"subitem_relation_name_text": "\u0026EMPTY\u0026"}], "subitem_relation_type_id": {"subitem_relation_type_id_text": "\u0026EMPTY\u0026", "subitem_relation_type_select": "URI"}}, {"subitem_relation_name": [{"subitem_relation_name_text": "\u0026EMPTY\u0026"}], "subitem_relation_type_id": {"subitem_relation_type_id_text": "\u0026EMPTY\u0026", "subitem_relation_type_select": "URI"}}, {"subitem_relation_name": [{"subitem_relation_name_text": "http://s-read.saitama-u.ac.jp/researchers/pages/researcher/QNzSsZBx"}], "subitem_relation_type_id": {"subitem_relation_type_id_text": "http://s-read.saitama-u.ac.jp/researchers/pages/researcher/QNzSsZBx", "subitem_relation_type_select": "URI"}}]}, "item_119_source_id_14": {"attribute_name": "ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "09145400", "subitem_source_identifier_type": "ISSN"}]}, "item_119_text_27": {"attribute_name": "版", "attribute_value_mlt": [{"subitem_text_value": "[出版社版]"}]}, "item_119_text_3": {"attribute_name": "著者 ローマ字", "attribute_value_mlt": [{"subitem_text_value": "LIOU, R., Chyuan"}, {"subitem_text_value": "MORI, Toshiyuki"}, {"subitem_text_value": "KOBAYASHI, Hidehiko"}, {"subitem_text_value": "MITAMURA, Takashi"}]}, "item_119_text_32": {"attribute_name": "アイテムID", "attribute_value_mlt": [{"subitem_text_value": "A1002256"}]}, "item_119_text_35": {"attribute_name": "公開日(XooNIps)", "attribute_value_mlt": [{"subitem_text_value": "Jan 9, 2008 09:00:00"}]}, "item_119_text_36": {"attribute_name": "最終更新日(XooNIps)", "attribute_value_mlt": [{"subitem_text_value": "Sep 8, 2009 13:24:30"}]}, "item_119_text_37": {"attribute_name": "更新履歴(XooNIps)", "attribute_value_mlt": [{"subitem_text_value": "Sep 8, 2009 フリーキーワード, 著者 を変更"}, {"subitem_text_value": "Mar 18, 2009 フリーキーワード, キーワード を変更"}, {"subitem_text_value": "Mar 18, 2009 フリーキーワード, キーワード を変更"}, {"subitem_text_value": "Oct 14, 2008 フリーキーワード, インデックス, キーワード を変更"}, {"subitem_text_value": "Mar 5, 2008 フリーキーワード, インデックス, キーワード を変更"}, {"subitem_text_value": "Feb 12, 2008 フリーキーワード, インデックス, キーワード を変更"}, {"subitem_text_value": "Jan 9, 2008 コメント, ID, フリーキーワード, インデックス, 版, キーワード を変更"}]}, "item_119_text_38": {"attribute_name": "登録者(XooNIps)", "attribute_value_mlt": [{"subitem_text_value": "sucra_jim4"}]}, "item_119_text_39": {"attribute_name": "閲覧数(XooNIps)", "attribute_value_mlt": [{"subitem_text_value": "1105"}]}, "item_119_text_4": {"attribute_name": "著者 所属", "attribute_value_mlt": [{"subitem_text_value": "埼玉大学工学部応用化学科"}, {"subitem_text_value": "東ソー(株)新材料研究所"}, {"subitem_text_value": "埼玉大学大学院理工学研究科物質科学部門"}, {"subitem_text_value": "埼玉大学工学部"}]}, "item_119_text_40": {"attribute_name": "ダウンロード数(XooNIps)", "attribute_value_mlt": [{"subitem_text_value": "361"}]}, "item_119_text_41": {"attribute_name": "XooNIps_インデックス", "attribute_value_mlt": [{"subitem_text_value": "sucra_jim4|Public/埼玉大学/理工学研究科|Public/埼玉大学/理工学研究科/物質科学部門|Public/主題別/化学/材料化学/無機工業材料|Public/ジャンル別/学術雑誌論文(国内)/日本セラミックス協会"}]}, "item_119_text_42": {"attribute_name": "XooNIps_ITEM_KEY", "attribute_value_mlt": [{"subitem_text_value": "1445"}]}, "item_119_text_5": {"attribute_name": "著者 所属(別言語)", "attribute_value_mlt": [{"subitem_text_value": "Department of Applied Chemistry, Faculty of Engineering, Saitama University"}, {"subitem_text_value": "Advanced Materials Research Laboratory, TOSOH Co. , Ltd."}, {"subitem_text_value": "Department of Applied Chemistry, Faculty of Engineering, Saitama University"}, {"subitem_text_value": "Department of Applied Chemistry, Faculty of Engineering, Saitama University"}]}, "item_119_text_9": {"attribute_name": "年月次", "attribute_value_mlt": [{"subitem_text_value": "1990-4"}]}, "item_119_version_type_28": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_version_resource": "http://purl.org/coar/version/c_970fb48d4fbd8a85", "subitem_version_type": "VoR"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "劉, 権栄"}, {"creatorName": "リュウ, チュアン", "creatorNameLang": "ja-Kana"}], "nameIdentifiers": [{"nameIdentifier": "20738", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "森, 利之"}, {"creatorName": "モリ, トシユキ", "creatorNameLang": "ja-Kana"}], "nameIdentifiers": [{"nameIdentifier": "20739", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "小林, 秀彦"}, {"creatorName": "コバヤシ, ヒデヒコ", "creatorNameLang": "ja-Kana"}], "nameIdentifiers": [{"nameIdentifier": "18337", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "三田村, 孝"}, {"creatorName": "ミタムラ, タカシ", "creatorNameLang": "ja-Kana"}], "nameIdentifiers": [{"nameIdentifier": "20740", "nameIdentifierScheme": "WEKO"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2018-01-24"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "A1002256.pdf", "filesize": [{"value": "2.2 MB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensetype": "license_free", "mimetype": "application/pdf", "size": 2200000.0, "url": {"label": "A1002256.pdf", "url": "https://sucra.repo.nii.ac.jp/record/13007/files/A1002256.pdf"}, "version_id": "7ba4afc0-536a-4927-8069-5f43eca4bf20"}]}, "item_keyword": {"attribute_name": "キーワード", "attribute_value_mlt": [{"subitem_subject": "Sintered Si_3N_4", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Corrosion", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Blast furnace slag", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Converter slag", "subitem_subject_scheme": "Other"}, {"subitem_subject": "O_2-N_2 atmosphere", "subitem_subject_scheme": "Other"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "jpn"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "journal article", "resourceuri": "http://purl.org/coar/resource_type/c_6501"}]}, "item_title": "鉄鋼スラグ及びその主成分に対するSi_3N_4焼結体の耐腐食性に及ぼす雰囲気の影響", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "鉄鋼スラグ及びその主成分に対するSi_3N_4焼結体の耐腐食性に及ぼす雰囲気の影響"}]}, "item_type_id": "119", "owner": "3", "path": ["426"], "permalink_uri": "https://sucra.repo.nii.ac.jp/records/13007", "pubdate": {"attribute_name": "公開日", "attribute_value": "2008-01-09"}, "publish_date": "2008-01-09", "publish_status": "0", "recid": "13007", "relation": {}, "relation_version_is_last": true, "title": ["鉄鋼スラグ及びその主成分に対するSi_3N_4焼結体の耐腐食性に及ぼす雰囲気の影響"], "weko_shared_id": -1}
鉄鋼スラグ及びその主成分に対するSi_3N_4焼結体の耐腐食性に及ぼす雰囲気の影響
https://sucra.repo.nii.ac.jp/records/13007
https://sucra.repo.nii.ac.jp/records/13007d5fdcbf9-b4e5-4877-965b-ee0a58f0d20f
名前 / ファイル | ライセンス | アクション |
---|---|---|
A1002256.pdf (2.2 MB)
|
|
Item type | 学術雑誌論文 / Journal Article(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2008-01-09 | |||||
タイトル | ||||||
タイトル | 鉄鋼スラグ及びその主成分に対するSi_3N_4焼結体の耐腐食性に及ぼす雰囲気の影響 | |||||
言語 | ||||||
言語 | jpn | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Sintered Si_3N_4 | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Corrosion | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Blast furnace slag | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Converter slag | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | O_2-N_2 atmosphere | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_6501 | |||||
資源タイプ | journal article | |||||
タイトル(別言語) | ||||||
その他のタイトル | Influence of Various Atmospheres on the Corrosion Resistance of Si_3N_4 Sintered Bodies against Steel Making Slag and Its Main Components | |||||
著者 |
劉, 権栄
× 劉, 権栄× 森, 利之× 小林, 秀彦× 三田村, 孝 |
|||||
著者 ローマ字 | ||||||
LIOU, R., Chyuan | ||||||
著者 ローマ字 | ||||||
MORI, Toshiyuki | ||||||
著者 ローマ字 | ||||||
KOBAYASHI, Hidehiko | ||||||
著者 ローマ字 | ||||||
MITAMURA, Takashi | ||||||
著者 所属 | ||||||
埼玉大学工学部応用化学科 | ||||||
著者 所属 | ||||||
東ソー(株)新材料研究所 | ||||||
著者 所属 | ||||||
埼玉大学大学院理工学研究科物質科学部門 | ||||||
著者 所属 | ||||||
埼玉大学工学部 | ||||||
著者 所属(別言語) | ||||||
Department of Applied Chemistry, Faculty of Engineering, Saitama University | ||||||
著者 所属(別言語) | ||||||
Advanced Materials Research Laboratory, TOSOH Co. , Ltd. | ||||||
著者 所属(別言語) | ||||||
Department of Applied Chemistry, Faculty of Engineering, Saitama University | ||||||
著者 所属(別言語) | ||||||
Department of Applied Chemistry, Faculty of Engineering, Saitama University | ||||||
書誌情報 |
日本セラミックス協会学術論文誌 巻 98, 号 1136, p. 348-354, 発行日 1990 |
|||||
年月次 | ||||||
1990-4 | ||||||
出版者名 | ||||||
出版者 | 社団法人日本セラミックス協会 | |||||
ISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 09145400 | |||||
関連サイト | ||||||
内容記述タイプ | Other | |||||
内容記述 | http://ci.nii.ac.jp/naid/110002289042/ | http://ci.nii.ac.jp/naid/110002289042/ | |||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | Corrosion of Si_3N_4 sintered bodies against blast furnace slags, converter slags and main components of these slags such as CaO, FeO and MnO_2 has been studied at 1200°-1400℃ for 1-12 h in air, Ar, N2 and O_2-N_2 atmospheres. For Si_3N_4 sintered bodies containing small amounts of Y_2O_3 and Al_2O_3 additives, the corrosion rate increased with increasing pores and glass phase in; sintered bodies. The corrosion behavior of Si_3N_4 sintered bodies against the various salts in Ar, N_2 and O_2-N_2 atmospheres, except for FeO salt, was very stable. In case of less corrosive salts such as blast furnace slag and CaO, the corrosion rate of Si_3N_4 sintered bodies in O_2-N_2 atmospheres increased with increasing O_2 partial pressure up to the air composition, the corrosion rate decreased extremely then above the air composition. In the corrosion of the Si_3N_4 sintered bodies against the various salts, the oxidation of Si3N4 seems to have occurred, and the corrosion proceeded continually by the reaction of SiO_2 with the salts | |||||
注記 | ||||||
内容記述タイプ | Other | |||||
内容記述 | rights: 社団法人日本セラミックス協会 rights: 本文データは学協会の許諾に基づきCiNiiから複製したものである relation: IsVersionOf: http://ci.nii.ac.jp/naid/110002289042/ |
|||||
版 | ||||||
[出版社版] | ||||||
著者版フラグ | ||||||
出版タイプ | VoR | |||||
出版タイプResource | http://purl.org/coar/version/c_970fb48d4fbd8a85 | |||||
資源タイプ | ||||||
内容記述タイプ | Other | |||||
内容記述 | text | |||||
フォーマット | ||||||
内容記述タイプ | Other | |||||
内容記述 | application/pdf | |||||
作成日 | ||||||
日付 | 2008-01-09 | |||||
日付タイプ | Created | |||||
アイテムID | ||||||
A1002256 |