{"_buckets": {"deposit": "817908c6-e43f-4b03-890d-354671375f99"}, "_deposit": {"created_by": 3, "id": "12977", "owners": [3], "pid": {"revision_id": 0, "type": "depid", "value": "12977"}, "status": "published"}, "_oai": {"id": "oai:sucra.repo.nii.ac.jp:00012977", "sets": ["426"]}, "author_link": ["20629", "20627", "20631", "20630", "20628"], "item_119_alternative_title_1": {"attribute_name": "タイトル(別言語)", "attribute_value_mlt": [{"subitem_alternative_title": "Changes of Microstructure and High-Temperature Strength of Ceramic Composite in the Mullite-ZrO_2-Al_2O_3 System Using an In-Situ Reaction between Synthetic Zircon and Ai_2O_3"}]}, "item_119_biblio_info_8": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "1994", "bibliographicIssueDateType": "Issued"}, "bibliographicIssueNumber": "1181", "bibliographicPageEnd": "98", "bibliographicPageStart": "93", "bibliographicVolumeNumber": "102", "bibliographic_titles": [{"bibliographic_title": "日本セラミックス協会学術論文誌"}]}]}, "item_119_date_31": {"attribute_name": "作成日", "attribute_value_mlt": [{"subitem_date_issued_datetime": "2008-01-09", "subitem_date_issued_type": "Created"}]}, "item_119_description_17": {"attribute_name": "関連サイト", "attribute_value_mlt": [{"subitem_description": "http://ci.nii.ac.jp/naid/110002290460/ | http://ci.nii.ac.jp/naid/110002290460/", "subitem_description_type": "Other"}]}, "item_119_description_19": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": "Ceramic composite was synthesized using an in situ reaction between synthetic zircon and Al_2O_3. High temperature strength did not decrease up to 1500℃ for the sample having only mullite for matrix. While, the strength decreased above 1300℃ for others. With in crease of the Al_2O_3 precipitated in the mullite matrix phase, the mullite grains became isotropic and small, which may occur the creep deformation. On the contrary, the ceramic composite used in the in situ reaction revealed excellent high temperature strength. It was found that ZrO_2 and Al_2O_3 particles dispersed in the grains of mullite matrix, contributed to increase the room temperature strength, and to improve effectively the high temperature strength. Remarkable difference of the microstructure was not observed in the composite obtained from the natural zircon instead of the synthetic zircon at same composition. However, high temperature strength decreased markedly due to the in crease of impurity content in the natural zircon. High temperature strength of the ceramic composite obtained from synthetic mullite, ZrO_2 and Al_2O_3 powders by the mixing method, decreased significantly at 1300℃. This behavior can be explained by the shape and size of the mullite in matrix, or the quantities of ZrO_2 and Al_2O_3 precipitated at the grain boundary.", "subitem_description_type": "Abstract"}]}, "item_119_description_21": {"attribute_name": "注記", "attribute_value_mlt": [{"subitem_description": "rights: 社団法人日本セラミックス協会\nrights: 本文データは学協会の許諾に基づきCiNiiから複製したものである\nrelation: IsVersionOf: http://ci.nii.ac.jp/naid/110002290460/", "subitem_description_type": "Other"}]}, "item_119_description_29": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"subitem_description": "text", "subitem_description_type": "Other"}]}, "item_119_description_30": {"attribute_name": "フォーマット", "attribute_value_mlt": [{"subitem_description": "application/pdf", "subitem_description_type": "Other"}]}, "item_119_publisher_11": {"attribute_name": "出版者名", "attribute_value_mlt": [{"subitem_publisher": "社団法人日本セラミックス協会"}]}, "item_119_source_id_14": {"attribute_name": "ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "09145400", "subitem_source_identifier_type": "ISSN"}]}, "item_119_text_27": {"attribute_name": "版", "attribute_value_mlt": [{"subitem_text_value": "[出版社版]"}]}, "item_119_text_3": {"attribute_name": "著者 ローマ字", "attribute_value_mlt": [{"subitem_text_value": "KUBOTA, Yoshitaka"}, {"subitem_text_value": "YAMAMOTO, Shigemi"}, {"subitem_text_value": "MORI, Toshiyuki"}, {"subitem_text_value": "YAMAMURA, Hiroshi"}, {"subitem_text_value": "MITAMURA, Takashi"}]}, "item_119_text_32": {"attribute_name": "アイテムID", "attribute_value_mlt": [{"subitem_text_value": "A1002227"}]}, "item_119_text_35": {"attribute_name": "公開日(XooNIps)", "attribute_value_mlt": [{"subitem_text_value": "Jan 9, 2008 09:00:00"}]}, "item_119_text_36": {"attribute_name": "最終更新日(XooNIps)", "attribute_value_mlt": [{"subitem_text_value": "Oct 13, 2008 20:49:08"}]}, "item_119_text_37": {"attribute_name": "更新履歴(XooNIps)", "attribute_value_mlt": [{"subitem_text_value": "Oct 13, 2008 フリーキーワード, インデックス, キーワード を変更"}, {"subitem_text_value": "Aug 8, 2008 フリーキーワード, キーワード を変更"}, {"subitem_text_value": "Mar 2, 2008 フリーキーワード, インデックス, キーワード を変更"}, {"subitem_text_value": "Feb 10, 2008 フリーキーワード, インデックス, キーワード を変更"}, {"subitem_text_value": "Jan 9, 2008 フリーキーワード, 版, キーワード を変更"}, {"subitem_text_value": "Jan 9, 2008 コメント, ID, フリーキーワード, インデックス, 版, キーワード を変更"}]}, "item_119_text_38": {"attribute_name": "登録者(XooNIps)", "attribute_value_mlt": [{"subitem_text_value": "sucra_jim4"}]}, "item_119_text_39": {"attribute_name": "閲覧数(XooNIps)", "attribute_value_mlt": [{"subitem_text_value": "927"}]}, "item_119_text_4": {"attribute_name": "著者 所属", "attribute_value_mlt": [{"subitem_text_value": "東ソー(株)筑波研究所"}, {"subitem_text_value": "東ソー(株)筑波研究所"}, {"subitem_text_value": "東ソー(株)筑波研究所"}, {"subitem_text_value": "東ソー(株)筑波研究所"}, {"subitem_text_value": "埼玉大学工学部"}]}, "item_119_text_40": {"attribute_name": "ダウンロード数(XooNIps)", "attribute_value_mlt": [{"subitem_text_value": "355"}]}, "item_119_text_41": {"attribute_name": "XooNIps_インデックス", "attribute_value_mlt": [{"subitem_text_value": "sucra_jim4|Public/埼玉大学/理工学研究科|Public/埼玉大学/理工学研究科/物質科学部門|Public/主題別/化学/材料化学/無機工業材料|Public/ジャンル別/学術雑誌論文(国内)/日本セラミックス協会"}]}, "item_119_text_42": {"attribute_name": "XooNIps_ITEM_KEY", "attribute_value_mlt": [{"subitem_text_value": "1415"}]}, "item_119_text_5": {"attribute_name": "著者 所属(別言語)", "attribute_value_mlt": [{"subitem_text_value": "Tsukuba Laboratory, TOSOH Co., Ltd."}, {"subitem_text_value": "Tsukuba Laboratory, TOSOH Co., Ltd."}, {"subitem_text_value": "Tsukuba Laboratory, TOSOH Co., Ltd."}, {"subitem_text_value": "Tsukuba Laboratory, TOSOH Co., Ltd."}, {"subitem_text_value": "Faculty of Engineering, Saitama University"}]}, "item_119_text_9": {"attribute_name": "年月次", "attribute_value_mlt": [{"subitem_text_value": "1994-1"}]}, "item_119_version_type_28": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_version_resource": "http://purl.org/coar/version/c_970fb48d4fbd8a85", "subitem_version_type": "VoR"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "窪田, 吉孝"}, {"creatorName": "クボタ, ヨシタカ", "creatorNameLang": "ja-Kana"}], "nameIdentifiers": [{"nameIdentifier": "20627", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "山本, 茂美"}, {"creatorName": "ヤマモト, シゲミ", "creatorNameLang": "ja-Kana"}], "nameIdentifiers": [{"nameIdentifier": "20628", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "森, 利之"}, {"creatorName": "モリ, トシユキ", "creatorNameLang": "ja-Kana"}], "nameIdentifiers": [{"nameIdentifier": "20629", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "山村, 博"}, {"creatorName": "ヤマムラ, ヒロシ", "creatorNameLang": "ja-Kana"}], "nameIdentifiers": [{"nameIdentifier": "20630", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "三田村, 孝"}, {"creatorName": "ミタムラ, タカシ", "creatorNameLang": "ja-Kana"}], "nameIdentifiers": [{"nameIdentifier": "20631", "nameIdentifierScheme": "WEKO"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2018-01-24"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "A1002227.pdf", "filesize": [{"value": "1.6 MB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensetype": "license_free", "mimetype": "application/pdf", "size": 1600000.0, "url": {"label": "A1002227.pdf", "url": "https://sucra.repo.nii.ac.jp/record/12977/files/A1002227.pdf"}, "version_id": "153a665c-6eec-40f7-acc2-ada8497d0efc"}]}, "item_keyword": {"attribute_name": "キーワード", "attribute_value_mlt": [{"subitem_subject": "Composite", "subitem_subject_scheme": "Other"}, {"subitem_subject": "High-temperature strength", "subitem_subject_scheme": "Other"}, {"subitem_subject": "In-situreaction", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Zircon", "subitem_subject_scheme": "Other"}, {"subitem_subject": "ZrO_2", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Al_2O_3", "subitem_subject_scheme": "Other"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "jpn"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "journal article", "resourceuri": "http://purl.org/coar/resource_type/c_6501"}]}, "item_title": "合成ジルコンとアルミナのin Situreactionを利用したムライト-ジルコニア-アルミナ系複合焼結体の徴構造変化と高温強度特性", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "合成ジルコンとアルミナのin Situreactionを利用したムライト-ジルコニア-アルミナ系複合焼結体の徴構造変化と高温強度特性"}]}, "item_type_id": "119", "owner": "3", "path": ["426"], "permalink_uri": "https://sucra.repo.nii.ac.jp/records/12977", "pubdate": {"attribute_name": "公開日", "attribute_value": "2008-01-09"}, "publish_date": "2008-01-09", "publish_status": "0", "recid": "12977", "relation": {}, "relation_version_is_last": true, "title": ["合成ジルコンとアルミナのin Situreactionを利用したムライト-ジルコニア-アルミナ系複合焼結体の徴構造変化と高温強度特性"], "weko_shared_id": -1}
合成ジルコンとアルミナのin Situreactionを利用したムライト-ジルコニア-アルミナ系複合焼結体の徴構造変化と高温強度特性
https://sucra.repo.nii.ac.jp/records/12977
https://sucra.repo.nii.ac.jp/records/12977a696f6e1-90a6-48f0-b88b-e8d03c19d4c6
名前 / ファイル | ライセンス | アクション |
---|---|---|
A1002227.pdf (1.6 MB)
|
|
Item type | 学術雑誌論文 / Journal Article(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2008-01-09 | |||||
タイトル | ||||||
タイトル | 合成ジルコンとアルミナのin Situreactionを利用したムライト-ジルコニア-アルミナ系複合焼結体の徴構造変化と高温強度特性 | |||||
言語 | ||||||
言語 | jpn | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Composite | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | High-temperature strength | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | In-situreaction | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Zircon | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | ZrO_2 | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | Al_2O_3 | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_6501 | |||||
資源タイプ | journal article | |||||
タイトル(別言語) | ||||||
その他のタイトル | Changes of Microstructure and High-Temperature Strength of Ceramic Composite in the Mullite-ZrO_2-Al_2O_3 System Using an In-Situ Reaction between Synthetic Zircon and Ai_2O_3 | |||||
著者 |
窪田, 吉孝
× 窪田, 吉孝× 山本, 茂美× 森, 利之× 山村, 博× 三田村, 孝 |
|||||
著者 ローマ字 | ||||||
KUBOTA, Yoshitaka | ||||||
著者 ローマ字 | ||||||
YAMAMOTO, Shigemi | ||||||
著者 ローマ字 | ||||||
MORI, Toshiyuki | ||||||
著者 ローマ字 | ||||||
YAMAMURA, Hiroshi | ||||||
著者 ローマ字 | ||||||
MITAMURA, Takashi | ||||||
著者 所属 | ||||||
東ソー(株)筑波研究所 | ||||||
著者 所属 | ||||||
東ソー(株)筑波研究所 | ||||||
著者 所属 | ||||||
東ソー(株)筑波研究所 | ||||||
著者 所属 | ||||||
東ソー(株)筑波研究所 | ||||||
著者 所属 | ||||||
埼玉大学工学部 | ||||||
著者 所属(別言語) | ||||||
Tsukuba Laboratory, TOSOH Co., Ltd. | ||||||
著者 所属(別言語) | ||||||
Tsukuba Laboratory, TOSOH Co., Ltd. | ||||||
著者 所属(別言語) | ||||||
Tsukuba Laboratory, TOSOH Co., Ltd. | ||||||
著者 所属(別言語) | ||||||
Tsukuba Laboratory, TOSOH Co., Ltd. | ||||||
著者 所属(別言語) | ||||||
Faculty of Engineering, Saitama University | ||||||
書誌情報 |
日本セラミックス協会学術論文誌 巻 102, 号 1181, p. 93-98, 発行日 1994 |
|||||
年月次 | ||||||
1994-1 | ||||||
出版者名 | ||||||
出版者 | 社団法人日本セラミックス協会 | |||||
ISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 09145400 | |||||
関連サイト | ||||||
内容記述タイプ | Other | |||||
内容記述 | http://ci.nii.ac.jp/naid/110002290460/ | http://ci.nii.ac.jp/naid/110002290460/ | |||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | Ceramic composite was synthesized using an in situ reaction between synthetic zircon and Al_2O_3. High temperature strength did not decrease up to 1500℃ for the sample having only mullite for matrix. While, the strength decreased above 1300℃ for others. With in crease of the Al_2O_3 precipitated in the mullite matrix phase, the mullite grains became isotropic and small, which may occur the creep deformation. On the contrary, the ceramic composite used in the in situ reaction revealed excellent high temperature strength. It was found that ZrO_2 and Al_2O_3 particles dispersed in the grains of mullite matrix, contributed to increase the room temperature strength, and to improve effectively the high temperature strength. Remarkable difference of the microstructure was not observed in the composite obtained from the natural zircon instead of the synthetic zircon at same composition. However, high temperature strength decreased markedly due to the in crease of impurity content in the natural zircon. High temperature strength of the ceramic composite obtained from synthetic mullite, ZrO_2 and Al_2O_3 powders by the mixing method, decreased significantly at 1300℃. This behavior can be explained by the shape and size of the mullite in matrix, or the quantities of ZrO_2 and Al_2O_3 precipitated at the grain boundary. | |||||
注記 | ||||||
内容記述タイプ | Other | |||||
内容記述 | rights: 社団法人日本セラミックス協会 rights: 本文データは学協会の許諾に基づきCiNiiから複製したものである relation: IsVersionOf: http://ci.nii.ac.jp/naid/110002290460/ |
|||||
版 | ||||||
[出版社版] | ||||||
著者版フラグ | ||||||
出版タイプ | VoR | |||||
出版タイプResource | http://purl.org/coar/version/c_970fb48d4fbd8a85 | |||||
資源タイプ | ||||||
内容記述タイプ | Other | |||||
内容記述 | text | |||||
フォーマット | ||||||
内容記述タイプ | Other | |||||
内容記述 | application/pdf | |||||
作成日 | ||||||
日付 | 2008-01-09 | |||||
日付タイプ | Created | |||||
アイテムID | ||||||
A1002227 |